Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.71 g/cm³ Show Supplier Material materials with Dichte of 2.71 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.2 - 3 mm Show Supplier Material materials with Dicke of 0.2 - 3 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegewinkel 180° | 23.0 °C | 1.5 °/t Show Supplier Material materials with Biegewinkel 180° of 1.5 °/t |
Biegewinkel 90° | 23.0 °C | 1 °/t Show Supplier Material materials with Biegewinkel 90° of 1 °/t |
Dehnung A50 | 23.0 °C | 2 - 3 % Show Supplier Material materials with Dehnung A50 of 2 - 3 % |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa |
Härte, HBW | 23.0 °C | 48 [-] Show Supplier Material materials with Härte, HBW of 48 [-] |
Schubmodule | 23.0 °C | 26.5 GPa Show Supplier Material materials with Schubmodule of 26.5 GPa |
Streckgrenze | 23.0 °C | 120 MPa Show Supplier Material materials with Streckgrenze of 120 MPa |
Zugfestigkeit | 23.0 °C | 145 - 185 MPa Show Supplier Material materials with Zugfestigkeit of 145 - 185 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 200 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 200 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 3.3E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.3E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 0.1 % Show Supplier Material materials with Chrom of 0.1 % |
Eisen | 0.7 % Show Supplier Material materials with Eisen of 0.7 % |
Kupfer | 0.2 % Show Supplier Material materials with Kupfer of 0.2 % |
Magnesium | 0.5 - 1.1 % Show Supplier Material materials with Magnesium of 0.5 - 1.1 % |
Mangan | 0.2 % Show Supplier Material materials with Mangan of 0.2 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Zink | 0.25 % Show Supplier Material materials with Zink of 0.25 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent (anodizing quality) | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Anodizing quality; Heat exchangers: Fins, General applications; Cosmetics: Cosmetics pieces; Automotive trim: Interior trim; Components: Automotive fins, Heat exchangers | |
Brazing | Good | |
Corrosion properties | Excellent | |
Welding | Very Good | |
Workability | Very Good |