Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.66 g/cm³ Show Supplier Material materials with Dichte of 2.66 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.2 - 6 mm Show Supplier Material materials with Dicke of 0.2 - 6 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 3 - 6 % Show Supplier Material materials with Dehnung A50 of 3 - 6 % |
Elastizitätsmodul | 23.0 °C | 71 GPa Show Supplier Material materials with Elastizitätsmodul of 71 GPa |
Härte, HBW | 23.0 °C | 81 [-] Show Supplier Material materials with Härte, HBW of 81 [-] |
Schubmodule | 23.0 °C | 27 GPa Show Supplier Material materials with Schubmodule of 27 GPa |
Streckgrenze | 23.0 °C | 200 MPa Show Supplier Material materials with Streckgrenze of 200 MPa |
Zugfestigkeit | 23.0 °C | 275 - 335 MPa Show Supplier Material materials with Zugfestigkeit of 275 - 335 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 126 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 126 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 5.6E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 5.6E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | 0.05 - 0.15 % Show Supplier Material materials with Andere of 0.05 - 0.15 % |
Chrom | 0.05 - 0.25 % Show Supplier Material materials with Chrom of 0.05 - 0.25 % |
Eisen | 0.5 % Show Supplier Material materials with Eisen of 0.5 % |
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % |
Magnesium | 3.5 - 4.5 % Show Supplier Material materials with Magnesium of 3.5 - 4.5 % |
Mangan | 0.2 - 0.7 % Show Supplier Material materials with Mangan of 0.2 - 0.7 % |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % |
Titan | 0.15 % Show Supplier Material materials with Titan of 0.15 % |
Zink | 0.25 % Show Supplier Material materials with Zink of 0.25 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent (anodizing quality) | |
Application areas | Vessels: Pressure, Cryogenics; Components: Access hatches, Spoilers, General tranportation | |
Corrosion properties | Excellent | |
Welding | Good | |
Workability | Good (in O temper) |