Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.69 g/cm³ Show Supplier Material materials with Dichte of 2.69 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.2 - 6 mm Show Supplier Material materials with Dicke of 0.2 - 6 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegewinkel 180° | 23.0 °C | 1.5 °/t Show Supplier Material materials with Biegewinkel 180° of 1.5 °/t |
Biegewinkel 90° | 23.0 °C | 0 - 1.5 °/t Show Supplier Material materials with Biegewinkel 90° of 0 - 1.5 °/t |
Dehnung A50 | 23.0 °C | 4 - 10 % Show Supplier Material materials with Dehnung A50 of 4 - 10 % |
Elastizitätsmodul | 23.0 °C | 68.6 GPa Show Supplier Material materials with Elastizitätsmodul of 68.6 GPa |
Härte, HBW | 23.0 °C | 56 [-] Show Supplier Material materials with Härte, HBW of 56 [-] |
Streckgrenze | 23.0 °C | 120 MPa Show Supplier Material materials with Streckgrenze of 120 MPa |
Zugfestigkeit | 23.0 °C | 190 - 230 MPa Show Supplier Material materials with Zugfestigkeit of 190 - 230 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 153 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 153 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 4.5E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.5E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | 0.05 - 0.15 % Show Supplier Material materials with Andere of 0.05 - 0.15 % |
Chrom | 0.15 % Show Supplier Material materials with Chrom of 0.15 % |
Eisen | 0.5 % Show Supplier Material materials with Eisen of 0.5 % |
Kupfer | 0.15 % Show Supplier Material materials with Kupfer of 0.15 % |
Magnesium | 1.7 - 2.4 % Show Supplier Material materials with Magnesium of 1.7 - 2.4 % |
Mangan | 0.1 - 0.5 % Show Supplier Material materials with Mangan of 0.1 - 0.5 % |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % |
Titan | 0.15 % Show Supplier Material materials with Titan of 0.15 % |
Zink | 0.15 % Show Supplier Material materials with Zink of 0.15 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Tubes: Industrial tubes, Pipes; Wind energy: Nacelle coverings, rotor hub, stairs; | |
Corrosion properties | Excellent | |
Welding | Very Good | |
Workability | Very Good |