Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.69 g/cm³ Show Supplier Material materials with Dichte of 2.69 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.3 - 1.2 mm Show Supplier Material materials with Dicke of 0.3 - 1.2 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 3 % Show Supplier Material materials with Dehnung A50 of 3 % |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa |
Schubmodule | 23.0 °C | 26.5 GPa Show Supplier Material materials with Schubmodule of 26.5 GPa |
Streckgrenze | 23.0 °C | 120 MPa Show Supplier Material materials with Streckgrenze of 120 MPa |
Zugfestigkeit | 23.0 °C | 170 - 190 MPa Show Supplier Material materials with Zugfestigkeit of 170 - 190 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 138 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 138 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 4.9E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.9E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | 0.05 % Show Supplier Material materials with Andere of 0.05 % |
Eisen | 0.1 % Show Supplier Material materials with Eisen of 0.1 % |
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % |
Magnesium | 0.6 - 1 % Show Supplier Material materials with Magnesium of 0.6 - 1 % |
Mangan | 0.03 % Show Supplier Material materials with Mangan of 0.03 % |
Silizium | 0.08 % Show Supplier Material materials with Silizium of 0.08 % |
Zink | 0.05 % Show Supplier Material materials with Zink of 0.05 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels; Anodizing quality; Cosmetics: Cosmetics pieces; Automotive trim: Interior trim, Window frame, Marque badges | |
Corrosion properties | Excellent | |
General machinability | Good | |
Welding | Good | |
Workability | Good |