Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.74 g/cm³ Show Supplier Material materials with Dichte of 2.74 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.06 - 0.2 mm Show Supplier Material materials with Dicke of 0.06 - 0.2 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 5 % Show Supplier Material materials with Dehnung A50 of 5 % |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa |
Schubmodule | 23.0 °C | 25 GPa Show Supplier Material materials with Schubmodule of 25 GPa |
Streckgrenze | 23.0 °C | 90 MPa Show Supplier Material materials with Streckgrenze of 90 MPa |
Zugfestigkeit | 23.0 °C | 110 - 170 MPa Show Supplier Material materials with Zugfestigkeit of 110 - 170 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 190 - 210 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 190 - 210 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 3.1E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.1E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Eisen | 1.2 - 2 % Show Supplier Material materials with Eisen of 1.2 - 2 % |
Kupfer | 0.3 % Show Supplier Material materials with Kupfer of 0.3 % |
Magnesium | 0.1 % Show Supplier Material materials with Magnesium of 0.1 % |
Mangan | 0.3 - 1 % Show Supplier Material materials with Mangan of 0.3 - 1 % |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % |
Zink | 0.1 % Show Supplier Material materials with Zink of 0.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Limited | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels; Roofing: Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels; Electronic devices: Housing of devices; Heat exchangers: Fins, Heat exchangers, General applications; Tubes: Industrial tubes, Flexible tubes, Pipes; Insulation; Semi-rigid and corrugated: Pet food, Smooth wall; Components: Automotive fins, Heat exchangers | |
Corrosion properties | Limited | |
Welding | Good | |
Workability | Very Good |