Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.71 g/cm³ Show Supplier Material materials with Dichte of 2.71 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.18 - 0.35 mm Show Supplier Material materials with Dicke of 0.18 - 0.35 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 2 % Show Supplier Material materials with Dehnung A50 of 2 % | according to EN 485-2 |
Elastizitätsmodul | 23.0 °C | 68.6 GPa Show Supplier Material materials with Elastizitätsmodul of 68.6 GPa | |
Schubmodule | 23.0 °C | 25.73 GPa Show Supplier Material materials with Schubmodule of 25.73 GPa | |
Streckgrenze | 23.0 °C | 110 - 140 MPa Show Supplier Material materials with Streckgrenze of 110 - 140 MPa | according to EN 485-2 |
Zugfestigkeit | 23.0 °C | 120 - 160 MPa Show Supplier Material materials with Zugfestigkeit of 120 - 160 MPa | according to EN 485-2 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 201 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 201 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 3E-8 - 3.5E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3E-8 - 3.5E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 0.1 % Show Supplier Material materials with Chrom of 0.1 % |
Eisen | 0.5 - 1 % Show Supplier Material materials with Eisen of 0.5 - 1 % |
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % |
Magnesium | 0.1 % Show Supplier Material materials with Magnesium of 0.1 % |
Mangan | 0.1 % Show Supplier Material materials with Mangan of 0.1 % |
Silizium | 0.4 - 0.8 % Show Supplier Material materials with Silizium of 0.4 - 0.8 % |
Titan | 0.05 % Show Supplier Material materials with Titan of 0.05 % |
Zink | 0.1 % Show Supplier Material materials with Zink of 0.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Interiors and ceilings: Sheets for mechanized panels; Furniture, Plinths, Blinds: Intermediate transformation/interior use; Heat exchangers: Fins, General applications; Tubes: Flexible tube, Pipes; Insulation; Closures: Long cups, Short cups, Easy open; Cosmetic: Cosmetic pieces; Pharmacy: Pharma and para-pharma; Semi-rigid and corrugated: Pet food, Smooth wall; Foil stock: Foil app | |
Corrosion properties | Moderated | |
Welding | Excellent | |
Workability | Excellent |