Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.73 g/cm³ Show Supplier Material materials with Dichte of 2.73 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.5 - 1 mm Show Supplier Material materials with Dicke of 0.5 - 1 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 25 % Show Supplier Material materials with Dehnung A50 of 25 % |
Elastizitätsmodul | 23.0 °C | 69 GPa Show Supplier Material materials with Elastizitätsmodul of 69 GPa |
Schubmodule | 23.0 °C | 26 GPa Show Supplier Material materials with Schubmodule of 26 GPa |
Streckgrenze | 23.0 °C | 40 - 70 MPa Show Supplier Material materials with Streckgrenze of 40 - 70 MPa |
Zugfestigkeit | 23.0 °C | 90 - 120 MPa Show Supplier Material materials with Zugfestigkeit of 90 - 120 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 120 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 120 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 3E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Eisen | 1.2 - 1.6 % Show Supplier Material materials with Eisen of 1.2 - 1.6 % |
Kupfer | 0.2 % Show Supplier Material materials with Kupfer of 0.2 % |
Magnesium | 0.1 % Show Supplier Material materials with Magnesium of 0.1 % |
Mangan | 0.2 - 0.6 % Show Supplier Material materials with Mangan of 0.2 - 0.6 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % |
Zink | 0.1 % Show Supplier Material materials with Zink of 0.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Good | |
Application areas | Semi-rigid and corrugated: Pet food; Automotive trim: Interior trim | |
Corrosion properties | Moderated | |
Welding | Excellent | |
Workability | Excellent |