Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.72 g/cm³ Show Supplier Material materials with Dichte of 2.72 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.09 - 0.14 mm Show Supplier Material materials with Dicke of 0.09 - 0.14 mm |
Mechanisch
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K |
Chemical properties
Property | Value |
---|---|
Chrom | 0.03 % Show Supplier Material materials with Chrom of 0.03 % |
Eisen | 1.1 - 1.7 % Show Supplier Material materials with Eisen of 1.1 - 1.7 % |
Kupfer | 0.05 % Show Supplier Material materials with Kupfer of 0.05 % |
Magnesium | 0.01 % Show Supplier Material materials with Magnesium of 0.01 % |
Mangan | 0.03 % Show Supplier Material materials with Mangan of 0.03 % |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % |
Titan | 0.05 % Show Supplier Material materials with Titan of 0.05 % |
Zink | 0.05 % Show Supplier Material materials with Zink of 0.05 % |
Technological properties
Property | ||
---|---|---|
Application areas | Foil stock: Foil app | |
Workability | Excellent |