Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.73 g/cm³ Show Supplier Material materials with Dichte of 2.73 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.08 - 0.2 mm Show Supplier Material materials with Dicke of 0.08 - 0.2 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 15 % Show Supplier Material materials with Dehnung A50 of 15 % |
Streckgrenze | 23.0 °C | 40 - 80 MPa Show Supplier Material materials with Streckgrenze of 40 - 80 MPa |
Zugfestigkeit | 23.0 °C | 110 - 150 MPa Show Supplier Material materials with Zugfestigkeit of 110 - 150 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.2 % Show Supplier Material materials with Chrom of 0.2 % |
Eisen | 0.6 - 1.2 % Show Supplier Material materials with Eisen of 0.6 - 1.2 % |
Kupfer | 0.3 % Show Supplier Material materials with Kupfer of 0.3 % |
Magnesium | 0.2 - 0.6 % Show Supplier Material materials with Magnesium of 0.2 - 0.6 % |
Mangan | 0.4 - 1 % Show Supplier Material materials with Mangan of 0.4 - 1 % |
Silizium | 0.6 % Show Supplier Material materials with Silizium of 0.6 % |
Zink | 0.25 % Show Supplier Material materials with Zink of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Semi-rigid and corrugated: Smooth wall |