Abmessung
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.01 % Show Supplier Material materials with Aluminium of 0.01 % | min. |
Bor | 0.001 % Show Supplier Material materials with Bor of 0.001 % | max. |
Chrom | 0.1 % Show Supplier Material materials with Chrom of 0.1 % | max. |
Kohlenstoff | 0.015 - 0.1 % Show Supplier Material materials with Kohlenstoff of 0.015 - 0.1 % | |
Kupfer | 0.15 % Show Supplier Material materials with Kupfer of 0.15 % | max. |
Mangan | 0.15 - 0.5 % Show Supplier Material materials with Mangan of 0.15 - 0.5 % | |
Nickel | 0.15 % Show Supplier Material materials with Nickel of 0.15 % | max. |
Niobium | 0.008 % Show Supplier Material materials with Niobium of 0.008 % | max. |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | max. |
Silizium | 0.03 % Show Supplier Material materials with Silizium of 0.03 % | max. |
Titan | 0.01 % Show Supplier Material materials with Titan of 0.01 % | max. |
Vanadium | 0.008 % Show Supplier Material materials with Vanadium of 0.008 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Steels for re-rolling are suitable, after processing, for cold forming by bending, drawing etc. They are also suitable for surface coating, with the exception of enamelling. Various examples of applications include: | |
Coating | Galvanisation: Class 1 | |
Heat Treatment | Batch annealing |