Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.18 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.18 [-] | max. |
Abmessung
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23 % Show Supplier Material materials with Dehnung of 23 % | min. | for thickness 1.5-2 mm | Transverse, A80 | |
24 % Show Supplier Material materials with Dehnung of 24 % | min. | for thickness 2-3 mm | Transverse, A80 | ||
28 % Show Supplier Material materials with Dehnung of 28 % | min. A5.65√So | for thickness 3-20 mm | ||
Kerbschlagenergie | 20 °C | 27 J Show Supplier Material materials with Kerbschlagenergie of 27 J | min. | for thickness 1.5-20 mm |
Streckgrenze | 240 - 360 MPa Show Supplier Material materials with Streckgrenze of 240 - 360 MPa | for thickness 1.5-2 mm | Transverse | |
240 - 340 MPa Show Supplier Material materials with Streckgrenze of 240 - 340 MPa | for thickness 2-20 mm | Transverse | ||
Zugfestigkeit | 360 - 430 MPa Show Supplier Material materials with Zugfestigkeit of 360 - 430 MPa | for thickness 1.5-20 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.01 % Show Supplier Material materials with Aluminium of 0.01 % | min. |
Kohlenstoff | 0.02 - 0.12 % Show Supplier Material materials with Kohlenstoff of 0.02 - 0.12 % | |
Mangan | 0.6 % Show Supplier Material materials with Mangan of 0.6 % | max. |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | max. |
Silizium | 0.03 % Show Supplier Material materials with Silizium of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Structural forming grade which is well suited to applications requiring high reproducibility of processing performance (especially control of springback). The S240D AM FCE grade is popular with Steel Service Centres, since it allows them to rationalise their supplies of deep drawable and structural steel. This grade is a versatile material for numerous applications in industry markets. | |
Chemical composition | The chemical properties given are based on cast analysis data. | |
Coating | Galvanisation: Class 1 |