Allgemein
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.35 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.35 [-] | max. |
Abmessung
Property | Value |
---|---|
Dimensions | For mill finish, coils in thicknesses greater than 20 mm can also be produced. Please contact us. Please feel free to check the figure on the right side of the material page for more details. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 17 % Show Supplier Material materials with Dehnung of 17 % | min. | for thickness 1.5-2 mm | Transverse, A80 | |
18 % Show Supplier Material materials with Dehnung of 18 % | min. | for thickness 2-2.5 mm | Transverse, A80 | ||
19 % Show Supplier Material materials with Dehnung of 19 % | min. | for thickness 2.5-3 mm | Transverse, A80 | ||
24 % Show Supplier Material materials with Dehnung of 24 % | min. A5.65√So | for thickness 3-20 mm | Transverse | ||
Kerbschlagenergie | 0 °C | 27 J Show Supplier Material materials with Kerbschlagenergie of 27 J | min. | for thickness 6-20 mm |
Streckgrenze | 225 MPa Show Supplier Material materials with Streckgrenze of 225 MPa | min. | for thickness 16-20 mm | Transverse | |
235 MPa Show Supplier Material materials with Streckgrenze of 235 MPa | min. | for thickness 1.5-16 mm | Transverse | ||
Zugfestigkeit | 360 - 510 MPa Show Supplier Material materials with Zugfestigkeit of 360 - 510 MPa | for thickness 1.5-20 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Kohlenstoff | 0.17 % Show Supplier Material materials with Kohlenstoff of 0.17 % | max. |
Kupfer | 0.55 % Show Supplier Material materials with Kupfer of 0.55 % | max. |
Mangan | 1.4 % Show Supplier Material materials with Mangan of 1.4 % | max. |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.03 % Show Supplier Material materials with Schwefel of 0.03 % | max. |
Silizium | 0.03 % Show Supplier Material materials with Silizium of 0.03 % | max. |
Stickstoff | 0.009 % Show Supplier Material materials with Stickstoff of 0.009 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Structural steels are mainly used in the building industry and in mechanical engineering. Applications include building components, containers, storage tanks and roll formed profiles. Since 1 July 2013, the Construction Products Regulation (Regulation (EU) No. 305/2011 – CPR) has required that CE marking be affixed to all products delivered in accordance with a harmonised standard (e.g. EN 10025). This CE marking guarantees, for the uses defined in the standard, the properties described in the declaration of performance submitted by the manufacturer. All of the steels in this data sheet comply with this Regulation. The corresponding declarations of performance are available on our website at http://dop.arcelormittal.net/index.php | |
Chemical composition | The above chemical properties are based on cast analysis data. | |
Coating | Galvanisation: Class 1 |