X42 AM FCE

Want to keep this datasheet? Save it now in your required format

Description

This steel is manufactured to the highest quality standards in order to meet the most stringent specifications. The reference standard is API 5L (American Petroleum Institute).

Special requirements such as HIC (hydrogen-induced cracking) resistance or high ductility at low temperature can be met to provide a solution for every pipeline project.

This steel for pipes has very high tensile strength and excellent toughness at very low temperatures and in heavy gauges. In addition, its special chemical composition with a particularly low carbon equivalent value gives it good weldability. The consistent mechanical properties of this steel improves its forming and welding performance.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von ArcelorMittal zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Allgemein

PropertyValueComment

Carbon equivalent (CEV)

0.4 [-]

Show Supplier Material materials with Carbon equivalent (CEV) of 0.4 [-]

max.

Abmessung

PropertyValue

Dimensions

For thicknesses over 20 mm, please contact us. Please feel free to check the figure on the right side of the material page for more details.

Mechanisch

PropertyTemperatureValueComment

Dehnung

21 %

Show Supplier Material materials with Dehnung of 21 %

min. | for thickness 5-25 mm | Transverse | A50

Drop-weight tear test

10 °C

100 %

Show Supplier Material materials with Drop-weight tear test of 100 %

min. | for thickness 5-25 mm

Kerbschlagenergie

0 °C

40 J

Show Supplier Material materials with Kerbschlagenergie of 40 J

min. | for thickness 5-25 mm | Transverse

Streckgrenze

290 - 495 MPa

Show Supplier Material materials with Streckgrenze of 290 - 495 MPa

for thickness 5-25 mm | Transverse

Yield to strength ratio

0.85 [-]

Show Supplier Material materials with Yield to strength ratio of 0.85 [-]

for thickness 5-25 mm | Transverse

Zugfestigkeit

415 - 585 MPa

Show Supplier Material materials with Zugfestigkeit of 415 - 585 MPa

for thickness 5-25 mm | Transverse

Chemical properties

PropertyValueComment

Aluminium

0.015 - 0.06 %

Show Supplier Material materials with Aluminium of 0.015 - 0.06 %

Chrom

0.3 %

Show Supplier Material materials with Chrom of 0.3 %

max.

Kohlenstoff

0.22 %

Show Supplier Material materials with Kohlenstoff of 0.22 %

max.

Kupfer

0.25 %

Show Supplier Material materials with Kupfer of 0.25 %

max.

Mangan

1.3 %

Show Supplier Material materials with Mangan of 1.3 %

max.

Molybdän

0.1 %

Show Supplier Material materials with Molybdän of 0.1 %

max.

Nickel

0.3 %

Show Supplier Material materials with Nickel of 0.3 %

max.

Niobium

0.05 %

Show Supplier Material materials with Niobium of 0.05 %

max.

Phosphor

0.025 %

Show Supplier Material materials with Phosphor of 0.025 %

max.

Schwefel

0.015 %

Show Supplier Material materials with Schwefel of 0.015 %

max.

Silizium

0.45 %

Show Supplier Material materials with Silizium of 0.45 %

max.

Stickstoff

0.012 %

Show Supplier Material materials with Stickstoff of 0.012 %

max.

Titan

0.04 %

Show Supplier Material materials with Titan of 0.04 %

max.

Vanadium

0.05 %

Show Supplier Material materials with Vanadium of 0.05 %

max.

Technological properties

Property
Application areas

ArcelorMittal's steels for pipes are particularly suitable for manufacturing:


  • Straight ERW pipes of up to 26” diameter
  • Spiral SAW pipes

    Spiral SAW and straight ERW pipes made with this type of steel are a good alternative to UOE pipes (made from plate from quarto roll mills) or seamless pipes.

    These steels are used for the production of pipes for the transport of gaseous or liquid materials such as water or oil.

  • Chemical composition

    Notes:

    1.A ratio Al/N ≥ 2 shall be applied.

    2. The sum of the percentages by mass of the three elements niobium, titanium and vanadium shall not exceed 0.15%.

    Hydrogen induced cracking

    HIC-resistant

    Since the dimensions available are constantly changing, please contact us for specific information.

    Other

    The mechanical properties of the pipes will depend on:


  • The Bauschinger effect, which in turn depends on
    • The grade and chemical composition of the steel
    • The type of pipe (ERW or SAW)
    • The type of pipe manufacturing line
  • The post-treatment (full body post-heating/stress relieving post-heating) that is sometimes performed by the client
  • The angle of the weld on spiral tubes (this will influence the direction of the tensile test with respect to the rolling direction)

    The evolution of the mechanical properties - and in particular of the difference in yield strength between the sheet and the pipe - is specific for each process. It is therefore very important to indicate both the forming and the welding process as well as the aforementioned sheet/pipe difference. An agreement between ArcelorMittal and the client on the coil mechanical properties to be guaranteed must be reached prior to delivery of the coils.

    The mechanical properties listed above are those of the pipes.

    The minimum elongation given above refers to a 610 mm diameter pipe with a wall thickness of 12.7 mm.

  • Welding

    The chemical composition of this steel ensures that there is no risk of cold cracking and simply applying the normal welding rules is sufficient to achieve a good quality weld. For SAW welding, the choice of an SA1 AM FCE flux/wire combination for grades up to X46 AM FCE, and an SA2 AM FCE for higher grades, should produce a weld with a coefficient greater than 1 and a good degree of toughness at the centre of the weld.