Allgemein
Property | Value | Comment |
---|---|---|
Mean Roughness | 0.6 - 1.9 μm Show Supplier Material materials with Mean Roughness of 0.6 - 1.9 μm | wide range of roughness levels according to the EN 10130 standard can be supplied upon request. |
Abmessung
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 26 % Show Supplier Material materials with Dehnung of 26 % | min. | for thickness 0.3-0.5 mm | Transverse | A80 |
28 % Show Supplier Material materials with Dehnung of 28 % | min. | for thickness 0.5-0.7 mm | Transverse | A80 | |
30 % Show Supplier Material materials with Dehnung of 30 % | min. | for thickness 0.7-3 mm | Transverse | A80 | |
Streckgrenze | 170 - 320 MPa Show Supplier Material materials with Streckgrenze of 170 - 320 MPa | for thickness 0.3-0.5 mm | Transverse |
170 - 300 MPa Show Supplier Material materials with Streckgrenze of 170 - 300 MPa | for thickness 0.5-0.7 mm | Transverse | |
170 - 280 MPa Show Supplier Material materials with Streckgrenze of 170 - 280 MPa | for thickness 0.7-3 mm | Transverse | |
Zugfestigkeit | 270 - 400 MPa Show Supplier Material materials with Zugfestigkeit of 270 - 400 MPa | for thickness 0.3-3 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | max. |
Kohlenstoff | 0.02 - 0.1 % Show Supplier Material materials with Kohlenstoff of 0.02 - 0.1 % | |
Mangan | 0.6 % Show Supplier Material materials with Mangan of 0.6 % | max. |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | max. |
Silizium | 0.03 % Show Supplier Material materials with Silizium of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Used for bending and deep drawing forming processes for applications where strength, rigidity and ductility are required. Typical applications are to be found in the automotive industry, the domestic appliance sector, metal furniture, drums, radiators, fans, small welded tubes and small profiles. Uncoated cold rolled steels for cold forming are suitable for food contact, under certain conditions laid down in the Regulation (EC) No. 1935/2004 and the French standard NF A 36-714. Please contact us for further information on this subject. | |
Coating | Galvanisation: Class 1 | |
Surface Finish | This grade is available in: | |
Surface condition | Surface cleanliness If improved surface cleanliness is required, ArcelorMittal also offers with compulsory use of hydrogen annealing. | |
Welding | Weldability is guaranteed when using the usual processes. Please specify which process you intend to use when ordering. | |
Workability | Forming limit curves can be used to define the maximum strains not to be exceeded when forming steel by various methods, so as to avoid the risk of incipient necking. These curves are available on request. |