Abmessung
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 26 % Show Supplier Material materials with Dehnung of 26 % | min. | for thickness 0.5-0.7 mm | Transverse | A80 |
28 % Show Supplier Material materials with Dehnung of 28 % | min. | for thickness 0.7-2 mm | Transverse | A80 | |
Streckgrenze | 140 - 300 MPa Show Supplier Material materials with Streckgrenze of 140 - 300 MPa | for thickness 0.5-0.7 mm | Transverse |
140 - 280 MPa Show Supplier Material materials with Streckgrenze of 140 - 280 MPa | for thickness 0.7-2 mm | Transverse | |
Zugfestigkeit | 270 - 410 MPa Show Supplier Material materials with Zugfestigkeit of 270 - 410 MPa | for thickness 0.5-2 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Kohlenstoff | 0.12 % Show Supplier Material materials with Kohlenstoff of 0.12 % | max. |
Mangan | 0.6 % Show Supplier Material materials with Mangan of 0.6 % | max. |
Phosphor | 0.045 % Show Supplier Material materials with Phosphor of 0.045 % | max. |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The main areas of use are: Blued steels are suitable for food contact, under certain conditions laid down in European Regulation (EC) No. 1935/2004 and French standard NF A 36-714. Please contact us for further information on this subject. | |
Coating | DC01BS AM FCE can be supplied with or without oil film. | |
Corrosion properties | Corrosion resistance is better than for uncoated cold rolled steels, but is nevertheless limited, particularly in humid atmospheres (salt spray test). | |
Processing methods | The processing conditions for DC01BS AM FCE is similar to those for cold forming. However, in the case of difficult drawing operations, the oxide layer may crack and lose its continuity. |