Abmessung
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mechanisch
Property | Value | Comment |
---|---|---|
Bend allowance | 0 [-] Show Supplier Material materials with Bend allowance of 0 [-] | min. | Transverse | for thickness 0.5-3 mm |
Dehnung | 24 % Show Supplier Material materials with Dehnung of 24 % | min. | for thickness 0.5-0.7 mm | A80 | Transverse |
25 % Show Supplier Material materials with Dehnung of 25 % | min. | for thickness 0.5-0.7 mm | A80 | |
26 % Show Supplier Material materials with Dehnung of 26 % | min. | for thickness 0.7-3 mm | A80 | Transverse | |
27 % Show Supplier Material materials with Dehnung of 27 % | min. | for thickness 0.7-3 mm | A80 | |
Streckgrenze | 240 - 310 MPa Show Supplier Material materials with Streckgrenze of 240 - 310 MPa | for thickness 0.5-3 mm |
260 - 330 MPa Show Supplier Material materials with Streckgrenze of 260 - 330 MPa | for thickness 0.5-3 mm | Transverse | |
Zugfestigkeit | 340 - 420 MPa Show Supplier Material materials with Zugfestigkeit of 340 - 420 MPa | for thickness 0.5-3 mm |
350 - 430 MPa Show Supplier Material materials with Zugfestigkeit of 350 - 430 MPa | for thickness 0.5-3 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.015 % Show Supplier Material materials with Aluminium of 0.015 % | min. |
Kohlenstoff | 0.08 % Show Supplier Material materials with Kohlenstoff of 0.08 % | max. |
Mangan | 0.6 % Show Supplier Material materials with Mangan of 0.6 % | max. |
Niobium | 0.09 % Show Supplier Material materials with Niobium of 0.09 % | max. |
Phosphor | 0.025 % Show Supplier Material materials with Phosphor of 0.025 % | max. |
Schwefel | 0.02 % Show Supplier Material materials with Schwefel of 0.02 % | max. |
Silizium | 0.03 % Show Supplier Material materials with Silizium of 0.03 % | max. |
Titan | 0.15 % Show Supplier Material materials with Titan of 0.15 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The steel grade is particularly suitable for structural parts that do not require severe forming (profiling, bending or light drawing): automotive structures and reinforcements, industrial shelving systems, radiators, racking systems, furniture, mechanical engineering applications etc. | |
Coating | Galvanisation: Class 1 | |
Surface condition | Surface cleanliness If improved surface cleanliness is required, ArcelorMittal also offers this steel grade with compulsory use of continuous annealing or hydrogen annealing. | |
Welding | The steel grade has good weldability in all welding processes. Based on many years’ practical experience in arc and resistance spot welding of its products, ArcelorMittal can provide valuable technical assistance in defining the welding parameters for this grade. | |
Workability | The deep drawing performance of the HC260LA AM FCE grade is equivalent to that of mild steel. Drawability decreases as the yield strength increases. Forming limit curves can be used to define the maximum strains not to be exceeded when forming steel by various methods, so as to avoid the risk of incipient necking. These curves are available on request. Please contact for other forming data on this grade for particular sheet thicknesses. |