Abmessung
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 15 % Show Supplier Material materials with Dehnung of 15 % | min. | for thickness 0.5-0.7 mm | A80 | Transverse |
16 % Show Supplier Material materials with Dehnung of 16 % | min. | for thickness 0.5-0.7 mm | A80 | |
17 % Show Supplier Material materials with Dehnung of 17 % | min. | for thickness 0.7-3 mm | A80 | Transverse | |
18 % Show Supplier Material materials with Dehnung of 18 % | min. | for thickness 0.7-3 mm | A80 | |
Streckgrenze | 390 - 500 MPa Show Supplier Material materials with Streckgrenze of 390 - 500 MPa | for thickness 0.5-3 mm |
420 - 520 MPa Show Supplier Material materials with Streckgrenze of 420 - 520 MPa | for thickness 0.5-3 mm | Transverse | |
Zugfestigkeit | 460 - 580 MPa Show Supplier Material materials with Zugfestigkeit of 460 - 580 MPa | for thickness 0.5-3 mm |
470 - 600 MPa Show Supplier Material materials with Zugfestigkeit of 470 - 600 MPa | for thickness 0.5-3 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.015 % Show Supplier Material materials with Aluminium of 0.015 % | min. |
Kohlenstoff | 0.14 % Show Supplier Material materials with Kohlenstoff of 0.14 % | max. |
Mangan | 1.6 % Show Supplier Material materials with Mangan of 1.6 % | max. |
Niobium | 0.09 % Show Supplier Material materials with Niobium of 0.09 % | max. |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | max. |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. |
Titan | 0.15 % Show Supplier Material materials with Titan of 0.15 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The steel grade is particularly suitable for structural parts that do not require severe forming (profiling, bending or light drawing): automotive structures and reinforcements, industrial shelving systems, radiators, racking systems, furniture, mechanical engineering applications etc. | |
Surface condition | Surface cleanliness If improved surface cleanliness is required, ArcelorMittal also offers this steel grade with compulsory use of continuous annealing or hydrogen annealing. | |
Welding | Based on many years’ practical experience in arc and resistance spot welding of its products, ArcelorMittal can provide valuable technical assistance in defining the welding parameters for this grade. | |
Workability | Forming limit curves can be used to define the maximum strains not to be exceeded when forming steel by various methods, so as to avoid the risk of incipient necking. These curves are available on request. Please contact for other forming data on this grade for particular sheet thicknesses. |