Abmessung
Property | Value |
---|---|
Dimensions | Please feel free to check the figure on the right side of the material page for more details. |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 32 % Show Supplier Material materials with Dehnung of 32 % | min. | for thickness 0.5-3 mm | Transverse | A80 |
Streckgrenze | 180 - 280 MPa Show Supplier Material materials with Streckgrenze of 180 - 280 MPa | for thickness 0.5-3 mm | Transverse |
Zugfestigkeit | 300 - 360 MPa Show Supplier Material materials with Zugfestigkeit of 300 - 360 MPa | for thickness 0.5-3 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | min. |
Kohlenstoff | 0.12 % Show Supplier Material materials with Kohlenstoff of 0.12 % | max. |
Mangan | 0.6 % Show Supplier Material materials with Mangan of 0.6 % | max. |
Phosphor | 0.03 % Show Supplier Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.025 % Show Supplier Material materials with Schwefel of 0.025 % | max. |
Silizium | 0.03 % Show Supplier Material materials with Silizium of 0.03 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | It is mainly used in general industry and in mechanical engineering. Applications include drums, building components, containers, storage tanks and roll formed profiles. | |
Coating | Galvanisation: Class 1 | |
Surface condition | Surface cleanliness If improved surface cleanliness is required, ArcelorMittal also offers this range with compulsory use of hydrogen annealing: HCxxxCS AM FCE grades. |