Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.75 g/cm³ Show Supplier Material materials with Dichte of 7.75 g/cm³ | for thickness 0.65 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 30 - 40 % Show Supplier Material materials with Dehnung of 30 - 40 % | for thickness 0.65 mm | Transverse | A80 |
Härte, Vickers | 140 - 170 [-] Show Supplier Material materials with Härte, Vickers of 140 - 170 [-] | for thickness 0.65 mm |
Number of bends | 5 [-] Show Supplier Material materials with Number of bends of 5 [-] | min. for thickness 0.65 mm | Guaranteed |
Streckgrenze | 270 - 320 MPa Show Supplier Material materials with Streckgrenze of 270 - 320 MPa | for thickness 0.65 mm | Transverse |
Yield to strength ratio | 0.62 - 0.67 [-] Show Supplier Material materials with Yield to strength ratio of 0.62 - 0.67 [-] | for thickness 0.65 mm |
Zugfestigkeit | 430 - 480 MPa Show Supplier Material materials with Zugfestigkeit of 430 - 480 MPa | for thickness 0.65 mm | Transverse |
Magnetisch
Property | Value | Frequency | Comment |
---|---|---|---|
Anisotropy of loss | 12 % Show Supplier Material materials with Anisotropy of loss of 12 % | (+/-) for thickness 0.65 mm | Guaranteed | |
Garantierte Polarisierung | 1.62 [-] Show Supplier Material materials with Garantierte Polarisierung of 1.62 [-] | min. | for thickness 0.65 mm | at 2500 A/m | |
1.72 [-] Show Supplier Material materials with Garantierte Polarisierung of 1.72 [-] | min. | for thickness 0.65 mm | Indicative | ||
1.83 [-] Show Supplier Material materials with Garantierte Polarisierung of 1.83 [-] | min. | for thickness 0.65 mm | at 10000 A/m | ||
Garantierter Kernverlust | 4.7 W/kg Show Supplier Material materials with Garantierter Kernverlust of 4.7 W/kg | 50Hz | max. for thickness 0.65 mm | at 1.5 T |
Stacking factor | 0.97 mm Show Supplier Material materials with Stacking factor of 0.97 mm | min. | for thickness 65 mm | Guaranteed | |
Typischer Kernverlust | 2.1 W/kg Show Supplier Material materials with Typischer Kernverlust of 2.1 W/kg | 50Hz | max. for thickness 0.65 mm | at 1 T |
6.13 W/kg Show Supplier Material materials with Typischer Kernverlust of 6.13 W/kg | 60Hz | max. for thickness 0.65 mm | at 1.5 T |
Technological properties
Property | ||
---|---|---|
Application areas | High permeability is particularly useful for applications such as ballasts and motors, because it makes it possible to build machines that meet the most stringent environmental regulations. High thermal conductivity is a significant advantage for large machines. | |
Coating | This high permeability grade is available non-insulated or varnished. | |
Other | The above properties are obtained without heat treatment after stamping. The material as supplied possesses all the required magnetic properties. |