Allgemein
Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.38 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.38 [-] | max. |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 21 % Show Supplier Material materials with Dehnung of 21 % | min. A5.65√So | for thickness 5-100 mm | Transverse | |
Kerbschlagenergie | 0 °C | 24 J Show Supplier Material materials with Kerbschlagenergie of 24 J | min. | for thickness 5-50 mm | Transverse |
0 °C | 27 J Show Supplier Material materials with Kerbschlagenergie of 27 J | min. | for thickness 50-70 mm | Transverse | |
0 °C | 34 J Show Supplier Material materials with Kerbschlagenergie of 34 J | min. | for thickness 5-50 mm | |
0 °C | 34 J Show Supplier Material materials with Kerbschlagenergie of 34 J | min. | for thickness 70-100 mm | Transverse | |
0 °C | 41 J Show Supplier Material materials with Kerbschlagenergie of 41 J | min. | for thickness 50-70 mm | |
0 °C | 50 J Show Supplier Material materials with Kerbschlagenergie of 50 J | min. | for thickness 70-100 mm | |
Streckgrenze | 355 MPa Show Supplier Material materials with Streckgrenze of 355 MPa | min. | for thickness 5-100 mm | Transverse | |
Zugfestigkeit | 490 - 630 MPa Show Supplier Material materials with Zugfestigkeit of 490 - 630 MPa | for thickness 5-100 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | min. |
Andere | 0.12 % Show Supplier Material materials with Andere of 0.12 % | max. | Nb + Ti + V |
Chrom | 0.2 % Show Supplier Material materials with Chrom of 0.2 % | max. |
Kohlenstoff | 0.18 % Show Supplier Material materials with Kohlenstoff of 0.18 % | max. |
Kupfer | 0.35 % Show Supplier Material materials with Kupfer of 0.35 % | max. |
Mangan | 0.9 - 1.6 % Show Supplier Material materials with Mangan of 0.9 - 1.6 % | |
Molybdän | 0.08 % Show Supplier Material materials with Molybdän of 0.08 % | max. |
Nickel | 0.4 % Show Supplier Material materials with Nickel of 0.4 % | max. |
Phosphor | 0.035 % Show Supplier Material materials with Phosphor of 0.035 % | max. |
Schwefel | 0.035 % Show Supplier Material materials with Schwefel of 0.035 % | max. |
Silizium | 0.5 % Show Supplier Material materials with Silizium of 0.5 % | max. |
Stickstoff | 0.012 % Show Supplier Material materials with Stickstoff of 0.012 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Steel for shipbuilding can be used for the entire range of shipbuilding applications e.g. for the hull and interior of ships | |
Delivery condtion | For the dimensions available please visit Dimension tables (see Table A). | |
Other | Agreements The maximum thickness approved in shipbuilding specifications can be communicated on request by your sales agent. Available options Options available (after prior agreement): Mechanical properties Charpy V notch impact test specimens should be taken in the longitudinal direction. Transverse test specimens are not usually required. Transverse test results for plates and wide flats should be guaranteed by the supplier. |