Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.79 g/cm³ Show Supplier Material materials with Dichte of 1.79 g/cm³ | dry | ISO 1183 |
Sauerstoffindex | 44 % Show Supplier Material materials with Sauerstoffindex of 44 % | dry | ISO 4589-1/-2 |
Wasserabsorption | 0.03 % Show Supplier Material materials with Wasserabsorption of 0.03 % | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | min. | nominal |
Elastizitätsmodul | 0.35 GPa Show Supplier Material materials with Elastizitätsmodul of 0.35 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 18 % Show Supplier Material materials with Elongation at yield of 18 % | dry | ISO 527-1/-2 | |
Streckgrenze | 10 MPa Show Supplier Material materials with Streckgrenze of 10 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Glasübergangstemperatur | -40 °C Show Supplier Material materials with Glasübergangstemperatur of -40 °C | dry | ISO 11357-1/-2 | 10°C/min | |||||
Schmelzpunkt | 122 °C Show Supplier Material materials with Schmelzpunkt of 122 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Wärmeformbeständigkeitstemperatur | 31 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 31 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
Entflammbarkeit | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 1 mm IEC 60695-11-10: V-0 and yellow card available |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 12 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 12 kV/mm | dry | IEC 60243-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzvolumenflussrate | 5.8 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 5.8 cm³/10min | dry | ISO 1133 | 232°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fluoropolymer Processing Aids | |
Certifications | Yellow Card |