Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Abrasion resistance | 40.5 mm³ Show Supplier Material materials with Abrasion resistance of 40.5 mm³ | dry | ISO 4649 |
Dichte | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.76 % Show Supplier Material materials with Moisture absorption of 0.76 % | Sim. to ISO 62 | |
Wasserabsorption | 1.43 % Show Supplier Material materials with Wasserabsorption of 1.43 % | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
Elastizitätsmodul | 0.7 GPa Show Supplier Material materials with Elastizitätsmodul of 0.7 GPa | cond. | ISO 527-1/-2 | ||
Elongation at yield | 17 % Show Supplier Material materials with Elongation at yield of 17 % | cond. | ISO 527-1/-2 | ||
Härte, Shore D | 66 [-] Show Supplier Material materials with Härte, Shore D of 66 [-] | dry | ISO 7619-1 | 15 seconds | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 19 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 19 kJ/m² | cond. | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Thermisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Healthcare-Other,IV Bags,Medical Catheters | |
Certifications | USP Class VI | |
Processing methods | Injection Molding: Extrusion: |