Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A5 | 23.0 °C | 10 % Show Supplier Material materials with Dehnung A5 of 10 % |
Härte, Brinell | 23.0 °C | 75 [-] Show Supplier Material materials with Härte, Brinell of 75 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 195 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 195 MPa |
Zugfestigkeit | 23.0 °C | 245 MPa Show Supplier Material materials with Zugfestigkeit of 245 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | balance |
Andere | 0.05 - 0.15 % Show Supplier Material materials with Andere of 0.05 - 0.15 % |
Chrom | 0.05 % Show Supplier Material materials with Chrom of 0.05 % |
Eisen | 0.1 - 0.3 % Show Supplier Material materials with Eisen of 0.1 - 0.3 % |
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % |
Magnesium | 0.35 - 0.6 % Show Supplier Material materials with Magnesium of 0.35 - 0.6 % |
Mangan | 0.1 % Show Supplier Material materials with Mangan of 0.1 % |
Silizium | 0.3 - 0.6 % Show Supplier Material materials with Silizium of 0.3 - 0.6 % |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % |
Zink | 0.15 % Show Supplier Material materials with Zink of 0.15 % |
Technological properties
Property | ||
---|---|---|
Coating | suitable for electro-chemical brightening and anodizing, for high decorative demands | |
Corrosion properties | corrosion resistant | |
Processing methods | excellent forming properties | |
Welding | weldable |