Chemical properties
Property | Value |
---|---|
Aluminium | balance |
Andere | 0.05 - 0.15 % Show Supplier Material materials with Andere of 0.05 - 0.15 % |
Chrom | 0.1 % Show Supplier Material materials with Chrom of 0.1 % |
Eisen | 0.35 % Show Supplier Material materials with Eisen of 0.35 % |
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % |
Magnesium | 0.4 - 0.6 % Show Supplier Material materials with Magnesium of 0.4 - 0.6 % |
Mangan | 0.1 % Show Supplier Material materials with Mangan of 0.1 % |
Silizium | 0.6 - 0.9 % Show Supplier Material materials with Silizium of 0.6 - 0.9 % |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % |
Zink | 0.1 % Show Supplier Material materials with Zink of 0.1 % |