Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 13.8 g/cm³ Show Supplier Material materials with Dichte of 13.8 g/cm³ | |
Binder | Cobalt binder | ||
Kornstruktur | Coarse grain size |
Mechanisch
Property | Temperature | Value |
---|---|---|
Druckfestigkeit | 23.0 °C | 3500 MPa Show Supplier Material materials with Druckfestigkeit of 3500 MPa |
Elastizitätsmodul | 23.0 °C | 510 GPa Show Supplier Material materials with Elastizitätsmodul of 510 GPa |
Härte, Rockwell A | 23.0 °C | 84.8 [-] Show Supplier Material materials with Härte, Rockwell A of 84.8 [-] |
Härte, Vickers, 10 | 23.0 °C | 910 [-] Show Supplier Material materials with Härte, Vickers, 10 of 910 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 23 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 23 MPa·√m |
Zugfestigkeit, transversal | 23.0 °C | 2850 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 2850 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.9E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.9E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 103 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 103 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Kobalt | 17.5 % Show Supplier Material materials with Kobalt of 17.5 % | as binder | |
Wolfram | WC balance |