Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 12.75 g/cm³ Show Supplier Material materials with Dichte of 12.75 g/cm³ | |
Binder | Cobalt binder | ||
Kornstruktur | Coarse grain size |
Mechanisch
Property | Temperature | Value |
---|---|---|
Druckfestigkeit | 23.0 °C | 3100 MPa Show Supplier Material materials with Druckfestigkeit of 3100 MPa |
Elastizitätsmodul | 23.0 °C | 420 GPa Show Supplier Material materials with Elastizitätsmodul of 420 GPa |
Härte, Rockwell A | 23.0 °C | 81.4 [-] Show Supplier Material materials with Härte, Rockwell A of 81.4 [-] |
Härte, Vickers, 10 | 23.0 °C | 690 [-] Show Supplier Material materials with Härte, Vickers, 10 of 690 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 27 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 27 MPa·√m |
Zugfestigkeit, transversal | 23.0 °C | 2700 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 2700 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.3E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.3E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 95 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 95 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Kobalt | 30 % Show Supplier Material materials with Kobalt of 30 % | as binder | |
Wolfram | WC balance |
Technological properties
Property |
---|