Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 14.5 g/cm³ Show Supplier Material materials with Dichte of 14.5 g/cm³ | |
Binder | Cobalt binder | ||
Kornstruktur | Fine grain size |
Mechanisch
Property | Temperature | Value |
---|---|---|
Druckfestigkeit | 23.0 °C | 6600 MPa Show Supplier Material materials with Druckfestigkeit of 6600 MPa |
Elastizitätsmodul | 23.0 °C | 585 GPa Show Supplier Material materials with Elastizitätsmodul of 585 GPa |
Härte, Rockwell A | 23.0 °C | 91.7 [-] Show Supplier Material materials with Härte, Rockwell A of 91.7 [-] |
Härte, Vickers | 23.0 °C | 1590 [-] Show Supplier Material materials with Härte, Vickers of 1590 [-] |
Plane-Strain Fracture Toughnes | 23.0 °C | 10.8 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 10.8 MPa·√m |
Zugfestigkeit, transversal | 23.0 °C | 3750 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 3750 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.3E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.3E-6 1/K |
Wärmeleitfähigkeit | 23.0 °C | 90 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 90 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Kobalt | 9.5 % Show Supplier Material materials with Kobalt of 9.5 % | as binder | |
Wolfram | WC balance |
Technological properties
Property |
---|