Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 14.8 g/cm³ Show Supplier Material materials with Dichte of 14.8 g/cm³ | |
Kornstruktur | Submicron (0,5µm - 0,8µm) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 624 GPa Show Supplier Material materials with Elastizitätsmodul of 624 GPa | |
Härte, Rockwell A | 23.0 °C | 93.2 [-] Show Supplier Material materials with Härte, Rockwell A of 93.2 [-] | |
Härte, Vickers, 10 | 23.0 °C | 1850 [-] Show Supplier Material materials with Härte, Vickers, 10 of 1850 [-] | EN ISO 6507-1 |
Härte, Vickers, 30 | 23.0 °C | 1820 [-] Show Supplier Material materials with Härte, Vickers, 30 of 1820 [-] | EN ISO 6507-1 |
Plane-Strain Fracture Toughnes | 23.0 °C | 9.3 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 9.3 MPa·√m | ISO 28079 |
Poissonzahl | 23.0 °C | 0.21 [-] Show Supplier Material materials with Poissonzahl of 0.21 [-] | |
Zugfestigkeit, transversal | 23.0 °C | 3600 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 3600 MPa | DIN EN ISO 7438 |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.8E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.8E-6 1/K |
Spezifische Wärmekapazität | 23.0 °C | 0.2 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 0.2 J/(kg·K) |
Temperaturleitfähigkeit | 23.0 °C | 24.4 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 24.4 mm²/s |
Wärmeleitfähigkeit | 23.0 °C | 73 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 73 W/(m·K) |
Chemical properties
Technological properties
Property |
---|