Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 13.84 g/cm³ Show Supplier Material materials with Dichte of 13.84 g/cm³ | |
Kornstruktur | Submicron (0,5µm - 0,8µm) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 512 GPa Show Supplier Material materials with Elastizitätsmodul of 512 GPa | |
Härte, Rockwell A | 23.0 °C | 90.5 [-] Show Supplier Material materials with Härte, Rockwell A of 90.5 [-] | |
Härte, Vickers, 10 | 23.0 °C | 1435 [-] Show Supplier Material materials with Härte, Vickers, 10 of 1435 [-] | EN ISO 6507-1 |
Härte, Vickers, 30 | 23.0 °C | 1415 [-] Show Supplier Material materials with Härte, Vickers, 30 of 1415 [-] | EN ISO 6507-1 |
Plane-Strain Fracture Toughnes | 23.0 °C | 13.2 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 13.2 MPa·√m | ISO 28079 |
Poissonzahl | 23.0 °C | 0.22 [-] Show Supplier Material materials with Poissonzahl of 0.22 [-] | |
Zugfestigkeit, transversal | 23.0 °C | 4300 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 4300 MPa | DIN EN ISO 7438 |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.7E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.7E-6 1/K |
Spezifische Wärmekapazität | 23.0 °C | 0.21 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 0.21 J/(kg·K) |
Temperaturleitfähigkeit | 23.0 °C | 18.8 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 18.8 mm²/s |
Wärmeleitfähigkeit | 23.0 °C | 55 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 55 W/(m·K) |
Chemical properties
Technological properties
Property |
---|