Allgemein
Property | Temperature | Value | |
---|---|---|---|
Dichte | 23.0 °C | 14.55 g/cm³ Show Supplier Material materials with Dichte of 14.55 g/cm³ | |
Kornstruktur | Ultrafine (0,2µm - 0,5µm) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 596 GPa Show Supplier Material materials with Elastizitätsmodul of 596 GPa | |
Härte, Rockwell A | 23.0 °C | 93.7 [-] Show Supplier Material materials with Härte, Rockwell A of 93.7 [-] | |
Härte, Vickers, 10 | 23.0 °C | 1970 [-] Show Supplier Material materials with Härte, Vickers, 10 of 1970 [-] | EN ISO 6507-1 |
Härte, Vickers, 30 | 23.0 °C | 1930 [-] Show Supplier Material materials with Härte, Vickers, 30 of 1930 [-] | EN ISO 6507-1 |
Plane-Strain Fracture Toughnes | 23.0 °C | 9.2 MPa·√m Show Supplier Material materials with Plane-Strain Fracture Toughnes of 9.2 MPa·√m | ISO 28079 |
Poissonzahl | 23.0 °C | 0.21 [-] Show Supplier Material materials with Poissonzahl of 0.21 [-] | |
Zugfestigkeit, transversal | 23.0 °C | 4400 MPa Show Supplier Material materials with Zugfestigkeit, transversal of 4400 MPa | DIN EN ISO 7438 |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.02E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.02E-6 1/K |
Chemical properties
Technological properties
Property |
---|