Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 0.9509 g/cm³ Show Supplier Material materials with Dichte of 0.9509 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.8 GPa Show Supplier Material materials with Biegemodul of 0.8 GPa | Min. |
Dehnung | 23.0 °C | 700 % Show Supplier Material materials with Dehnung of 700 % | |
Härte, Shore D | 23.0 °C | 62 [-] Show Supplier Material materials with Härte, Shore D of 62 [-] | |
Zugfestigkeit | 23.0 °C | 26 MPa Show Supplier Material materials with Zugfestigkeit of 26 MPa |
Thermisch
Property | Value | Comment |
---|---|---|
Brittleness temperature | -70 °C Show Supplier Material materials with Brittleness temperature of -70 °C | Max. |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Oberflächenisolierungswiderstand | 23.0 °C | 1.00E+16 Ω·cm² Show Supplier Material materials with Oberflächenisolierungswiderstand of 1.00E+16 Ω·cm² | Min., GOST 50499 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 0.3 - 0.7 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 0.3 - 0.7 g/10min | GOST 11645, 190°С/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | METALEN PE-11K is used in the cable manufacture as a jacket of power cables and optical communication cables. | |
Processing methods | Temperature profile: Zone 1: 140°С, Zone 2: 150°С, Zone 3: 170°С, Zone 4: 180°С, Die plate: 200°С. |