Alloy 36 (Invar®) Controlled Expansion Alloy

View suppliers (21)
Want to keep this datasheet? Save it now in your required format

Description

1.3912 (FeNi36) is a 36% nickel-iron alloy. It exhibits a near zero rate of thermal expansion from around –100°C up to 200°C. This is around a tenth of the expansion rate of carbon steels. Alloy 36 also demonstrates a high retention of strength and toughness at cryogenic temperatures, making it suitable for a variety of low temperature or low expansion applications. The alloy is ideally suited to areas where dimensional changes due to temperature must be minimal, such as tooling for aerospace composites, radio and electronic devices and structural members in precision equipment such as lasers, measuring devices, thermostats and cryogenic instrumentation. Alloy 36 can also be utilised in combination with a high expansion material to crate mechanical movement with temperature in thermomechanical controls and switchgear.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

23.0 °C

8.13 g/cm³

Show Material materials with Dichte of 8.13 g/cm³

Mechanisch

PropertyTemperatureValue

Dehnung

23.0 °C

30 %

Show Material materials with Dehnung of 30 %

Elastizitätsmodul

23.0 °C

140 GPa

Show Material materials with Elastizitätsmodul of 140 GPa

Härte, Vickers

23.0 °C

140 [-]

Show Material materials with Härte, Vickers of 140 [-]

Streckgrenze

23.0 °C

310 MPa

Show Material materials with Streckgrenze of 310 MPa

Zugfestigkeit

23.0 °C

480 MPa

Show Material materials with Zugfestigkeit of 480 MPa

Thermisch

PropertyTemperatureValue

Koeffizient der thermischen Ausdehnung

30.0 °C

1.2E-6 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-6 1/K

150.0 °C

2.7E-6 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.7E-6 1/K

Schmelzpunkt

1450 °C

Show Material materials with Schmelzpunkt of 1450 °C

Spezifische Wärmekapazität

23.0 °C

510 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 510 J/(kg·K)

Wärmeleitfähigkeit

23.0 °C

10.5 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 10.5 W/(m·K)

Chemical properties

PropertyValue

Eisen

63 %

Show Material materials with Eisen of 63 %

Mangan

0.6 %

Show Material materials with Mangan of 0.6 %

Nickel

36 %

Show Material materials with Nickel of 36 %

Silizium

0.4 %

Show Material materials with Silizium of 0.4 %

Technological properties

Property
Application areas

General: Positioning devices, bimetal thermostats, advanced composite moulds for aerospace industry, optical devices, echo boxes and filters for mobile telephones, magnetic shielding, small electrical transformers, metrology devices, scientific instruments, electrical circuit breakers, temperature regulators, clock balance wheels, pendulum clocks, precision condenser blades, radar and microwave cavity resonators, special electronic housings, seals, spacers, and specialized frames, high voltage transmission lines