Das Material: 'NIBRON SPECIAL® Copper Alloy', nach dem Sie gesucht haben, wurde durch das untenstehende ersetzt.

NIBRON SPECIAL® Copper Alloy

View suppliers (1)
Want to keep this datasheet? Save it now in your required format

Description

2.1504 (CuNi14Al3) is an extra high strength copper nickel alloy developed by Columbia Metals that maximises both strength and corrosion resistance. Sometimes referred to as a nickel bronze, NIBRON® contains additions of aluminium, iron and manganese that join with the copper and nickel to achieve its exceptional properties. Although suited primarily to the tough extremes of marine or offshore oil and gas environments, Nibron® has also established itself for critical components in many other industrial sectors including aerospace, electrical, chemical and automotive. It shows the following features and properties:


  • Very high mechanical properties
  • Excellent wear and galling resistance
  • High ductility
  • Outstanding resistance to marine corrosion and erosion
  • Retention of properties at cryogenic temperatures
  • Exceptionally low magnetic permeability
  • Good machinability and dimensional stability
  • Good thermal conductivity
  • Equivalent Materials

    Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Eigenschaften

    Allgemein

    PropertyTemperatureValue

    Dichte

    23.0 °C

    8.5 g/cm³

    Show Material materials with Dichte of 8.5 g/cm³

    Mechanisch

    PropertyTemperatureValue

    Dehnung

    23.0 °C

    12 %

    Show Material materials with Dehnung of 12 %

    Elastizitätsmodul

    23.0 °C

    141 GPa

    Show Material materials with Elastizitätsmodul of 141 GPa

    Härte, Brinell

    23.0 °C

    229 - 240 [-]

    Show Material materials with Härte, Brinell of 229 - 240 [-]

    Streckgrenze Rp 0,2

    23.0 °C

    555 - 630 MPa

    Show Material materials with Streckgrenze Rp 0,2 of 555 - 630 MPa

    Zugfestigkeit

    23.0 °C

    770 - 850 MPa

    Show Material materials with Zugfestigkeit of 770 - 850 MPa

    Thermisch

    PropertyTemperatureValueComment

    Koeffizient der thermischen Ausdehnung

    23.0 °C

    1.64E-5 1/K

    Show Material materials with Koeffizient der thermischen Ausdehnung of 1.64E-5 1/K

    for 0-400°C

    Schmelzpunkt

    1080 - 1100 °C

    Show Material materials with Schmelzpunkt of 1080 - 1100 °C

    Wärmeleitfähigkeit

    23.0 °C

    44 - 46 W/(m·K)

    Show Material materials with Wärmeleitfähigkeit of 44 - 46 W/(m·K)

    Elektrisch

    PropertyTemperatureValue

    spezifischer Widerstand

    23.0 °C

    1.7E-7 Ω·m

    Show Material materials with spezifischer Widerstand of 1.7E-7 Ω·m

    Magnetisch

    PropertyTemperatureValueComment

    Relative magnetische Permeabilität

    23.0 °C

    1 [-]

    Show Material materials with Relative magnetische Permeabilität of 1 [-]

    max.

    Chemical properties

    PropertyValue

    Aluminium

    3 %

    Show Material materials with Aluminium of 3 %

    Eisen

    1.5 %

    Show Material materials with Eisen of 1.5 %

    Kupfer

    Balance

    Mangan

    0.3 %

    Show Material materials with Mangan of 0.3 %

    Nickel

    14.5 %

    Show Material materials with Nickel of 14.5 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Marine shafts and bearing bushes, offshore bolting, valve and pump trim;Aerospace: Aircraft landing gear bushes, actuating sleeves, steering gear, bearing bushes, non-magnetic bolts and control surface components;Automotive: High performance engine shafts, gears, pinions, bearing bushes, locking nuts, mechanical and electromechanical components, thrust washers and hydraulic equipment;Chemical processing: Pump and valve spindles and other trim, flanges, pipe fittings, clamps and plant components

    Corrosion properties

    Excellent corrosion resistance

    General machinability

    Good machinability