Description

2.0857 (CuNi3Si) ultimate super strength copper nickel silicon alloy, specially developed to provide a unique blend of mechnical and physical properties for high performance engineering. It has similar characteristics to Colsibro®, although Trojan is produced with increased levels of nickel and silicon in order to further increase the mechanical strength. It shows the following features and properties:


  • Ultra-high strength
  • High electrical and thermal conductivity
  • Excellent wear and galling resistance
  • Extremely low magnetic permeability
  • Excellent general corrosion resistance
  • Outstanding bearing properties
  • Spark resistance
  • Good machinability and dimensional stability
  • Outstanding low temperature mechanical properties
  • Related Standards

    Equivalent Materials

    Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    Eigenschaften

    Allgemein

    PropertyTemperatureValue

    Dichte

    23.0 °C

    8.8 g/cm³

    Show Material materials with Dichte of 8.8 g/cm³

    Mechanisch

    PropertyTemperatureValue

    Dehnung

    23.0 °C

    10 %

    Show Material materials with Dehnung of 10 %

    Härte, Brinell

    23.0 °C

    190 - 200 [-]

    Show Material materials with Härte, Brinell of 190 - 200 [-]

    Streckgrenze Rp 0,2

    23.0 °C

    570 - 750 MPa

    Show Material materials with Streckgrenze Rp 0,2 of 570 - 750 MPa

    Zugfestigkeit

    23.0 °C

    690 - 800 MPa

    Show Material materials with Zugfestigkeit of 690 - 800 MPa

    Thermisch

    PropertyTemperatureValueComment

    Koeffizient der thermischen Ausdehnung

    23.0 °C

    1.6E-5 1/K

    Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K

    for 0-400°C

    Schmelzpunkt

    1060 - 1085 °C

    Show Material materials with Schmelzpunkt of 1060 - 1085 °C

    Wärmeleitfähigkeit

    23.0 °C

    159 W/(m·K)

    Show Material materials with Wärmeleitfähigkeit of 159 W/(m·K)

    Elektrisch

    PropertyTemperatureValue

    Elektrische Leitfähigkeit

    23.0 °C

    1.74E+7 S/m

    Show Material materials with Elektrische Leitfähigkeit of 1.74E+7 S/m

    Specific Electrical conductivity

    30 % IACS

    Show Material materials with Specific Electrical conductivity of 30 % IACS

    Magnetisch

    PropertyTemperatureValue

    Relative magnetische Permeabilität

    23.0 °C

    1 [-]

    Show Material materials with Relative magnetische Permeabilität of 1 [-]

    Chemical properties

    PropertyValue

    Kupfer

    Balance

    Nickel

    2.6 - 4.5 %

    Show Material materials with Nickel of 2.6 - 4.5 %

    Silizium

    0.8 - 1.3 %

    Show Material materials with Silizium of 0.8 - 1.3 %

    Technological properties

    Property
    Application areas

    Automotive: valve guides, bushes and valve seats;Electrical: current-carrying electrical components such as slip rings, squirrel cages, springs, rotary switch contacts, contact blades, short-circuit rings and heavy duty switchgear;Offshore & marine: Downhole tools, shear pins, hydraulic valve bodies, pump components and ball valves and mechanical seals;Other: Non-magnetic tooling, plastic mould tooling, friction pads and fibre optic connectors

    Corrosion properties

    Excellent corrosion resistance

    General machinability

    Good machinability