Description

2.4668 (NiCr19NbMo) is a precipitation hardening nickel-chromium alloy that also contains additions of iron, niobium, molybdenum, aluminium and titanium, providing a unique combination of high strength and corrosion resistance together with excellent weldability. It shows the following features and properties:


  • Excellent tensile, fatigue, creep and rupture strengths across a wide temperature range from around -253ºC to 705ºC
  • Excellent oxidation resistance, up to temperatures of around 980ºC due to the high chromium content
  • Outstanding corrosion resistance in many environments including organic and inorganic acids, other than when strongly oxidising, hydrogen sulphide and sour gases
  • Especially resistant to chloride stress-corrosion cracking
  • Exceptional weldability
  • Related Standards

    Equivalent Materials

    Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Eigenschaften

    Allgemein

    PropertyTemperatureValue

    Dichte

    23.0 °C

    8.22 g/cm³

    Show Material materials with Dichte of 8.22 g/cm³

    Mechanisch

    PropertyTemperatureValue

    Dehnung

    23.0 °C

    12 - 17 %

    Show Material materials with Dehnung of 12 - 17 %

    Elastizitätsmodul

    23.0 °C

    204 GPa

    Show Material materials with Elastizitätsmodul of 204 GPa

    Flächenreduzierung

    23.0 °C

    15 %

    Show Material materials with Flächenreduzierung of 15 %

    Härte, Brinell

    23.0 °C

    313 - 354 [-]

    Show Material materials with Härte, Brinell of 313 - 354 [-]

    Streckgrenze Rp 0,2

    23.0 °C

    827 - 1034 MPa

    Show Material materials with Streckgrenze Rp 0,2 of 827 - 1034 MPa

    Zugfestigkeit

    23.0 °C

    1034 - 1276 MPa

    Show Material materials with Zugfestigkeit of 1034 - 1276 MPa

    Thermisch

    PropertyTemperatureValueComment

    Koeffizient der thermischen Ausdehnung

    23.0 °C

    1.35E-5 1/K

    Show Material materials with Koeffizient der thermischen Ausdehnung of 1.35E-5 1/K

    Schmelzpunkt

    1260 - 1335 °C

    Show Material materials with Schmelzpunkt of 1260 - 1335 °C

    Wärmeleitfähigkeit

    23.0 °C

    14.2 W/(m·K)

    Show Material materials with Wärmeleitfähigkeit of 14.2 W/(m·K)

    for 0-200°C

    Magnetisch

    PropertyTemperatureValue

    Relative magnetische Permeabilität

    23.0 °C

    1 [-]

    Show Material materials with Relative magnetische Permeabilität of 1 [-]

    Chemical properties

    PropertyValue

    Aluminium

    0.5 %

    Show Material materials with Aluminium of 0.5 %

    Chrom

    19 %

    Show Material materials with Chrom of 19 %

    Eisen

    18 - 18.5 %

    Show Material materials with Eisen of 18 - 18.5 %

    Molybdän

    3 %

    Show Material materials with Molybdän of 3 %

    Nickel

    53 %

    Show Material materials with Nickel of 53 %

    Niobium

    5 %

    Show Material materials with Niobium of 5 %

    Titan

    0.9 %

    Show Material materials with Titan of 0.9 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Fasteners, valves, choke stems, down-hole tooling, cryogenic storage tanks and pump bodies;Aerospace: Jet engine components, rocket motors and thrust reversers;Power generation: Nuclear reactor parts, gas turbine components, nuclear fuel element spacers, containment vessels and valves;Other: Hot extrusion tooling

    Corrosion properties

    Excellent corrosion resistance

    Hot forming

    It can be hot worked between 985-1150°C.