2.4819 (NiMo16Cr15W) is a wrought nickel-chromium-molybdenum-tungsten alloy which displays remarkable corrosion resistance in a very wide range of processing environments. It offers excellent resistance to stress corrosion cracking and oxidising atmospheres up to 1040°C, whilst the high molybdenum content gives the alloy its excellent resistance to pitting and crevice corrosion. The low carbon content prevents the formation of grain boundary precipitates during welding. It shows the following features and properties:


  • Excellent resistance to pitting and corrosion
  • High mechanical properties
  • Excellent resistance to oxidising atmospheres up to 1040°C
  • Very high resistance to many aggressive chemicals
  • Related Standards

    Equivalent Materials

    Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    Eigenschaften

    Mechanisch

    PropertyTemperatureValue

    Dehnung

    23.0 °C

    40 %

    Show Material materials with Dehnung of 40 %

    Streckgrenze Rp 0,2

    23.0 °C

    283 MPa

    Show Material materials with Streckgrenze Rp 0,2 of 283 MPa

    Zugfestigkeit

    23.0 °C

    690 MPa

    Show Material materials with Zugfestigkeit of 690 MPa

    Chemical properties

    PropertyValue

    Chrom

    15.5 %

    Show Material materials with Chrom of 15.5 %

    Eisen

    5.5 %

    Show Material materials with Eisen of 5.5 %

    Molybdän

    16 %

    Show Material materials with Molybdän of 16 %

    Nickel

    57 %

    Show Material materials with Nickel of 57 %

    Wolfram

    3.8 %

    Show Material materials with Wolfram of 3.8 %

    Technological properties

    Property
    Application areas

    Chemical processing: Arduous areas of flue gas desulphurisation plants, critical components in sewage treatment, chemical and petrochemical plants, waste incineration, sour gas production and organic acid processing

    Corrosion properties

    Excellent corrosion resistance