Description

2.4360 (NiCu30Fe) is a nickel-copper alloy resistant to seawater and steam at high temperatures and widely used in the chemical, oil and marine industries. As a solution strengthened material, Monel Alloy 400 displays good strength, toughness and corrosion resistance at temperatures up to 400°C. It is supplied by Columbia Metals in the cold worked condition as standard. It shows the following features and properties:


  • Good strength and toughness
  • Excellent corrosion resistance in marine environments
  • Good resistance to non oxidising acids, alkalis and salts
  • Not susceptible to chloride stress corrosion cracking
  • Readily weldable
  • Related Standards

    Equivalent Materials

    Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

    Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
    Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Eigenschaften

    Allgemein

    PropertyTemperatureValue

    Dichte

    23.0 °C

    8.8 g/cm³

    Show Material materials with Dichte of 8.8 g/cm³

    Mechanisch

    PropertyTemperatureValueComment

    Dehnung

    23.0 °C

    20 - 35 %

    Show Material materials with Dehnung of 20 - 35 %

    Elastizitätsmodul

    23.0 °C

    180 GPa

    Show Material materials with Elastizitätsmodul of 180 GPa

    Härte, Rockwell C

    23.0 °C

    35 [-]

    Show Material materials with Härte, Rockwell C of 35 [-]

    max.

    Streckgrenze Rp 0,2

    23.0 °C

    170 - 415 MPa

    Show Material materials with Streckgrenze Rp 0,2 of 170 - 415 MPa

    Zugfestigkeit

    23.0 °C

    480 - 600 MPa

    Show Material materials with Zugfestigkeit of 480 - 600 MPa

    Thermisch

    PropertyTemperatureValue

    Koeffizient der thermischen Ausdehnung

    23.0 °C

    1.39E-5 1/K

    Show Material materials with Koeffizient der thermischen Ausdehnung of 1.39E-5 1/K

    Schmelzpunkt

    1300 - 1350 °C

    Show Material materials with Schmelzpunkt of 1300 - 1350 °C

    Wärmeleitfähigkeit

    23.0 °C

    22 W/(m·K)

    Show Material materials with Wärmeleitfähigkeit of 22 W/(m·K)

    Elektrisch

    PropertyValue

    Specific Electrical conductivity

    34 % IACS

    Show Material materials with Specific Electrical conductivity of 34 % IACS

    Chemical properties

    PropertyValueComment

    Eisen

    2.5 %

    Show Material materials with Eisen of 2.5 %

    max.

    Kupfer

    28 - 34 %

    Show Material materials with Kupfer of 28 - 34 %

    Mangan

    2 %

    Show Material materials with Mangan of 2 %

    Nickel

    63 %

    Show Material materials with Nickel of 63 %

    min., (Ni+Co)

    Technological properties

    Property
    Application areas

    Offshore & marine: Marine components, shafts, splash zone sheathing and fasteners;Chemical processing: Components for the manufacture of chlorinated solvents, salt production, ethyl chloride purification and numerous other areas of process plant;Other: Wire netting for insulation, oil well recovery pumps and crude oil distillation towers

    Cold Forming

    It can be cold worked

    Corrosion properties

    Excellent corrosion resistance in marine environments

    General machinability

    It is readily machinable

    Hot forming

    It can be hot worked