Abmessung
Property | Value |
---|---|
Breite | 1010 mm Show Supplier Material materials with Breite of 1010 mm |
Dicke | 20 - 400 mm Show Supplier Material materials with Dicke of 20 - 400 mm |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Brinell | 280 - 325 [-] Show Supplier Material materials with Härte, Brinell of 280 - 325 [-] | as-delivered condition |
Härte, Rockwell C | 28 - 51 [-] Show Supplier Material materials with Härte, Rockwell C of 28 - 51 [-] | |
Zugfestigkeit | 950 - 1095 MPa Show Supplier Material materials with Zugfestigkeit of 950 - 1095 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100 °C | 1.23e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.23e-05 1/K | for 20°C to the mentioned temperature | Quenched and Tempered |
200 °C | 1.3e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.3e-05 1/K | for 20°C to the mentioned temperature | Quenched and Tempered | |
300 °C | 1.37e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.37e-05 1/K | for 20°C to the mentioned temperature | Quenched and Tempered | |
Wärmeleitfähigkeit | 100 °C | 39.8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 39.8 W/(m·K) | |
150 °C | 40.4 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 40.4 W/(m·K) | ||
200 °C | 40.4 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 40.4 W/(m·K) | ||
250 °C | 39.9 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 39.9 W/(m·K) | ||
300 °C | 39 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 39 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 1.9 % Show Supplier Material materials with Chrom of 1.9 % |
Eisen | Balance |
Kohlenstoff | 0.4 % Show Supplier Material materials with Kohlenstoff of 0.4 % |
Mangan | 1.5 % Show Supplier Material materials with Mangan of 1.5 % |
Molybdän | 0.2 % Show Supplier Material materials with Molybdän of 0.2 % |
Schwefel | 0.05 % Show Supplier Material materials with Schwefel of 0.05 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Mould frames for plastic and die casting moulds, press brake dies, plastic moulds without special requirements on surface quality. | |
Heat Treatment | Soft annealing: 710-740°C (Cooling in furnace) - Stress relief annealing cooling in furnace (annealed): approx 600°C - Stress relief annealing cooling in furnace (quenched and tempered): approx 30-50°C under tempering temperature - Hardening: 840-870°C and quenching in oil or salt bath T=180-220°C |