Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 165 MPa Show Supplier Material materials with Biegefestigkeit of 165 MPa | ISO 178 |
Dehnung | 23.0 °C | 1.2 % Show Supplier Material materials with Dehnung of 1.2 % | ISO 178 |
Elastizitätsmodul | 23.0 °C | 18 GPa Show Supplier Material materials with Elastizitätsmodul of 18 GPa | ISO 178 (Flexural Test) |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 3.8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3.8 kJ/m² | ISO 179-1 |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 16 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 16 kJ/m² | ISO 179-1 |
Zugfestigkeit | 23.0 °C | 80 MPa Show Supplier Material materials with Zugfestigkeit of 80 MPa | ISO 527 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Glasübergangstemperatur | 160 °C Show Supplier Material materials with Glasübergangstemperatur of 160 °C | ISO 6721-7 | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | ISO 11359-2, Mean value for 20-105°C |
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | UL 746 (Flexural Test) | |
Wärmeleitfähigkeit | 23.0 °C | 0.85 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.85 W/(m·K) | ISO 8894 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 50Hz | 23.0 °C | 5.2 [-] Show Supplier Material materials with Dielectric constant, 50Hz of 5.2 [-] | IEC 60250 |
Durchschlagfestigkeit | 23.0 °C | 23 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 23 kV/mm | IEC 60243-1, 3mm Plate |
Kriechstromfestigkeit | 23.0 °C | 275 V Show Supplier Material materials with Kriechstromfestigkeit of 275 V | IEC 60112 |
Loss tangent, 50Hz | 23.0 °C | 1.1 [-] Show Supplier Material materials with Loss tangent, 50Hz of 1.1 [-] | IEC 60250 |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Encapsulation of electrical devices e.g. Protection of PCB, Solenoids, Sensors | |
Fillers | Glass Fiber |