Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.95 g/cm³ Show Supplier Material materials with Dichte of 1.95 g/cm³ | DIN 53479 |
Wasserabsorption | 23.0 °C | 0.06 % Show Supplier Material materials with Wasserabsorption of 0.06 % | ISO 62, 100°C/30 min |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 190 MPa Show Supplier Material materials with Biegefestigkeit of 190 MPa | ISO 178 |
Dehnung | 23.0 °C | 1.4 % Show Supplier Material materials with Dehnung of 1.4 % | ISO 178 |
Elastizitätsmodul | 23.0 °C | 17 GPa Show Supplier Material materials with Elastizitätsmodul of 17 GPa | ISO 178 (Flexural Test) |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 22 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 22 kJ/m² | ISO 179-1 |
Zugfestigkeit | 23.0 °C | 100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | ISO 527 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Glasübergangstemperatur | 120 °C Show Supplier Material materials with Glasübergangstemperatur of 120 °C | ISO 6721-7 | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2E-5 1/K | ISO 11359-2, Mean value for 20-105°C |
Wärmeleitfähigkeit | 23.0 °C | 0.85 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.85 W/(m·K) | ISO 8894 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 50Hz | 23.0 °C | 5 [-] Show Supplier Material materials with Dielectric constant, 50Hz of 5 [-] | IEC 60250 |
Kriechstromfestigkeit | 23.0 °C | 300 V Show Supplier Material materials with Kriechstromfestigkeit of 300 V | IEC 60112 |
Loss tangent, 50Hz | 23.0 °C | 1.6 [-] Show Supplier Material materials with Loss tangent, 50Hz of 1.6 [-] | IEC 60250 |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Encapsulation of electrical devices, e.g. Electronic, Sensors, Solenoids, Stators | |
Fillers | Glass Fiber |