Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 2.25 g/cm³ Show Supplier Material materials with Dichte of 2.25 g/cm³ | DIN 53479 |
Wasserabsorption | 23.0 °C | 0.03 % Show Supplier Material materials with Wasserabsorption of 0.03 % | ISO 62, 100°C/30 min |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 125 MPa Show Supplier Material materials with Biegefestigkeit of 125 MPa | ISO 178 |
Dehnung | 23.0 °C | 0.8 % Show Supplier Material materials with Dehnung of 0.8 % | ISO 178 |
Elastizitätsmodul | 23.0 °C | 18 GPa Show Supplier Material materials with Elastizitätsmodul of 18 GPa | ISO 178 (Flexural Test) |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 8 kJ/m² | ISO 179-1 |
Zugfestigkeit | 23.0 °C | 70 MPa Show Supplier Material materials with Zugfestigkeit of 70 MPa | ISO 527 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Glasübergangstemperatur | 160 °C Show Supplier Material materials with Glasübergangstemperatur of 160 °C | ISO 6721 | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | TMA |
Wärmeleitfähigkeit | 23.0 °C | 1.4 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 1.4 W/(m·K) | ISO 8894 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 50Hz | 23.0 °C | 5.8 [-] Show Supplier Material materials with Dielectric constant, 50Hz of 5.8 [-] | IEC 60250 |
Durchschlagfestigkeit | 23.0 °C | 19 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 19 kV/mm | IEC 60243-1, 3mm Plate |
Kriechstromfestigkeit | 23.0 °C | 425 V Show Supplier Material materials with Kriechstromfestigkeit of 425 V | IEC 60112 |
Loss tangent, 50Hz | 23.0 °C | 1.5 [-] Show Supplier Material materials with Loss tangent, 50Hz of 1.5 [-] | IEC 60250 |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | For applications with high heat dissipation e.g. electronic coatings, rotors, stators etc. |