Allgemein
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 25 °C | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | ISO 1183-1 | |
Low volatile organic compounds emissions | 23 °C | 10 μg/g Show Supplier Material materials with Low volatile organic compounds emissions of 10 μg/g | VDA 278 | max. |
Total volatile organic compounds emissions | 23 °C | 15 μgC/g Show Supplier Material materials with Total volatile organic compounds emissions of 15 μgC/g | VDA 277 | max. |
Volatile organic compounds emissions | 23 °C | 10 μg/g Show Supplier Material materials with Volatile organic compounds emissions of 10 μg/g | VDA 278 | max. |
Wasserabsorption | 0.2 % Show Supplier Material materials with Wasserabsorption of 0.2 % | ISO 62 | 23 °C | 50 % r.h., Equilibrium | |
0.7 % Show Supplier Material materials with Wasserabsorption of 0.7 % | ISO 62 | Water at 23 °C, Saturation |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Biegefestigkeit | 85 MPa Show Supplier Material materials with Biegefestigkeit of 85 MPa | ISO 178 | 2 mm/min | |
Biegemodul | 2.3 GPa Show Supplier Material materials with Biegemodul of 2.3 GPa | ISO 178 | 2 mm/min | |
Dehnung | 70 % Show Supplier Material materials with Dehnung of 70 % | ISO 527-1/2 | 50 mm/min | |
Elastizitätsmodul | 2.3 GPa Show Supplier Material materials with Elastizitätsmodul of 2.3 GPa | ISO 527-1/2 | 1 mm/min | |
Elongation at yield | 4.7 % Show Supplier Material materials with Elongation at yield of 4.7 % | ISO 527-1/2 | 50 mm/min | |
Schlagzähigkeit, Izod gekerbt | -40 °C | 30 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 30 kJ/m² | ISO 180-1A | |
-30 °C | 39 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 39 kJ/m² | ISO 180-1A | ||
23 °C | 53 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 53 kJ/m² | ISO 180-1A | ||
Streckgrenze | 55 MPa Show Supplier Material materials with Streckgrenze of 55 MPa | ISO 527-1/2 | 50 mm/min |
Thermisch
Property | Value | Testing Standard | Pressure | Comment | |||
---|---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 7.7e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.7e-05 1/K | ISO 11359-1/2 | 23 to 55°C | ||||
8.1e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.1e-05 1/K | ISO 11359-1/2 | 23 to 55°C, Transverse | |||||
Vicat-Erweichungstemperatur | 128 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 128 °C | ISO 306 | B50 | 50°C/h | ||||
130 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 130 °C | ISO 306 | B120 | 120°C/h | |||||
Wärmeformbeständigkeitstemperatur | 104 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 104 °C | ISO 75-1/2 | 1.8 MPa | ||||
123 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 123 °C | ISO 75-1/2 | 0.45 MPa | |||||
Entflammbarkeit | At thickness 1.6 mm UL 94: HB. Burning rate US-FMVSS (150x105x1 mm): < 80 mm/min according to ISO 3795 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 21 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 21 cm³/10min | ISO 1133 | 260°C/5Kg |
Schrumpfung | 0.65 - 0.75 % Show Supplier Material materials with Schrumpfung of 0.65 - 0.75 % | ISO 294-4 | 60x60x2 mm |
0.65 - 0.75 % Show Supplier Material materials with Schrumpfung of 0.65 - 0.75 % | ISO 294-4 | 60x60x2 mm, Transverse |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Chemical composition | Thermoplastic polymer blend based on polycarbonate (PC) and acrylonitrile-butadiene-styrene (ABS). | |
Color | White to slightly yellowish. | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |