Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Biegefestigkeit | 70 MPa Show Supplier Material materials with Biegefestigkeit of 70 MPa | ISO 178 | 2 mm/min | |
Biegemodul | 2.4 GPa Show Supplier Material materials with Biegemodul of 2.4 GPa | ISO 527-1/2 | 2 mm/min | |
Dehnung | 15 % Show Supplier Material materials with Dehnung of 15 % | ISO 527-1/2 | min. | 50 mm/min | |
Elastizitätsmodul | 2.4 GPa Show Supplier Material materials with Elastizitätsmodul of 2.4 GPa | ISO 527-1/2 | 1 mm/min | |
Elongation at yield | 2.6 % Show Supplier Material materials with Elongation at yield of 2.6 % | ISO 527-1/2 | 50 mm/min | |
Hardness, Ball Indentation | 110 MPa Show Supplier Material materials with Hardness, Ball Indentation of 110 MPa | ISO 2039-1 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | ISO 179-1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | ISO 179-1eA | ||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 90 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m² | ISO 179-1eU | |
23 °C | 110 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 110 kJ/m² | ISO 179-1eU | ||
Schlagzähigkeit, Izod gekerbt | -30 °C | 7 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 7 kJ/m² | ISO 180-1A | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 15 kJ/m² | ISO 180-1A | ||
Streckgrenze | 46 MPa Show Supplier Material materials with Streckgrenze of 46 MPa | ISO 527-1/2 | 50 mm/min |
Thermisch
Property | Value | Testing Standard | Pressure | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | IEC 60695-2-12 | 2.0 mm | ||||
Koeffizient der thermischen Ausdehnung | 9e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-05 1/K | ISO 11359-1/2 | 23 to 55°C | ||||
Vicat-Erweichungstemperatur | 99 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 99 °C | ISO 306 | 50 N | 50°C/h | ||||
Wärmeformbeständigkeitstemperatur | 94 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 94 °C | ISO 75-1/2 | 1.8 MPa | ||||
98 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 98 °C | ISO 75-1/2 | 0.45 MPa | |||||
Entflammbarkeit | At thickness 1.6 mm UL 94: HB. Burning rate US-FMVSS (200x105x2 mm): 60 mm/min according to ISO 3795 |
Elektrisch
Property | Value | Frequency | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 2.9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 2.9 [-] | 1MHz | IEC 60250 | |
3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3 [-] | 100Hz | IEC 60250 | ||
Durchschlagfestigkeit | 35 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 35 kV/mm | IEC 60243-1 | 1 mm | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 | Solution A | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | |||
Verlustfaktor | 0.005 [-] Show Supplier Material materials with Verlustfaktor of 0.005 [-] | 100Hz | IEC 60250 | |
0.008 [-] Show Supplier Material materials with Verlustfaktor of 0.008 [-] | 1MHz | IEC 60250 | ||
Volume resistivity | 1e+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+15 Ω·cm | IEC 60093 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 31 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 31 cm³/10min | ISO 1133 | 220°C/10Kg |
Schrumpfung | 0.4 - 0.7 % Show Supplier Material materials with Schrumpfung of 0.4 - 0.7 % | ISO 294-4 | 60x60x2 mm |
0.4 - 0.7 % Show Supplier Material materials with Schrumpfung of 0.4 - 0.7 % | ISO 294-4 | 60x60x2 mm, Transverse |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |
Other | Control measurements in other places may issue different results due to influences of machinery, equipment, test method or storage conditions. | |
Processing methods | Injection molding-melt temperature: 240 ºC according to ISO 294 Injection molding-mold temperature: 70 ºC according to ISO 294 Injection molding-injection velocity: 240 mm/s according to ISO 294 |