Allgemein
Property | Value |
---|---|
Dichte | 1.26 g/cm³ Show Supplier Material materials with Dichte of 1.26 g/cm³ |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dehnung | 120 % Show Supplier Material materials with Dehnung of 120 % | DIN EN ISO 527-1 | 50 mm/min |
Elastizitätsmodul | 0.185 GPa Show Supplier Material materials with Elastizitätsmodul of 0.185 GPa | DIN EN ISO 527-1 | 50 mm/min |
Schlagzähigkeit, Charpy ungekerbt | No Break | DIN EN ISO 179-1eU | |
Zugfestigkeit | 10 MPa Show Supplier Material materials with Zugfestigkeit of 10 MPa | DIN EN ISO 527-1 | 50 mm/min |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Glasübergangstemperatur | -100 °C Show Supplier Material materials with Glasübergangstemperatur of -100 °C | DIN 53765 | |
Max. Betriebstemperatur | 70 °C Show Supplier Material materials with Max. Betriebstemperatur of 70 °C | Long | |
100 °C Show Supplier Material materials with Max. Betriebstemperatur of 100 °C | Short | ||
Schmelzpunkt | 109 °C Show Supplier Material materials with Schmelzpunkt of 109 °C |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 19 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 19 g/10min | DIN EN ISO 1133 | 280°C/5kg |
Schmelzvolumenflussrate | 18 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 18 cm³/10min | DIN EN ISO 1133 | 230°C/5kg |
Schrumpfung | 1.84 % Show Supplier Material materials with Schrumpfung of 1.84 % | DIN EN ISO 294-4 | Transverse |
3 % Show Supplier Material materials with Schrumpfung of 3 % | DIN EN ISO 294-4 |
Technological properties
Property | ||
---|---|---|
Certifications | FDA compliant | |
Color | Blue | |
Detectability | Inductive: 6 mm Al, X-Ray detectable: 3.5 mm Al | |
Fillers | Mineral Powder | |
Processing methods | Permissible residual moisture content (%): 0.1, drying temperature (°C): 80, drying time (h): 4, mould temperature (°C): 40, material temperature (°C): 240, cylinder/processing temperature (°C): 240 |