Allgemein
Property | Value | Testing Standard | Comment |
---|---|---|---|
Dichte | 1.28 g/cm³ Show Supplier Material materials with Dichte of 1.28 g/cm³ | ||
Schüttdichte | 0.68 g/cm³ Show Supplier Material materials with Schüttdichte of 0.68 g/cm³ | EN ISO 60 | |
Wasserabsorption | 0.1 % Show Supplier Material materials with Wasserabsorption of 0.1 % | DIN EN ISO 62 | 23°C | 50 % r.h. up to saturation |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit | 43 MPa Show Supplier Material materials with Biegefestigkeit of 43 MPa | DIN EN ISO 178 | |
Biegemodul | 1.8 GPa Show Supplier Material materials with Biegemodul of 1.8 GPa | DIN EN ISO 178 | |
Dehnung | 30 % Show Supplier Material materials with Dehnung of 30 % | DIN EN ISO 527-1 | 50 mm/min |
Elastizitätsmodul | 2.2 GPa Show Supplier Material materials with Elastizitätsmodul of 2.2 GPa | DIN EN ISO 527-1 | 50 mm/min |
Flexural strain | 5 % Show Supplier Material materials with Flexural strain of 5 % | DIN EN ISO 178 | |
Schlagzähigkeit, Charpy ungekerbt | 20 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 20 kJ/m² | DIN EN ISO 179-1eU | |
Zugfestigkeit | 25 MPa Show Supplier Material materials with Zugfestigkeit of 25 MPa | DIN EN ISO 527-1 | 50 mm/min |
Thermisch
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Glasübergangstemperatur | 13 °C Show Supplier Material materials with Glasübergangstemperatur of 13 °C | ||||
Max. Betriebstemperatur | 100 °C Show Supplier Material materials with Max. Betriebstemperatur of 100 °C | Long | |||
130 °C Show Supplier Material materials with Max. Betriebstemperatur of 130 °C | Short | ||||
Schmelzpunkt | 165 °C Show Supplier Material materials with Schmelzpunkt of 165 °C | DIN 53765 | |||
Entflammbarkeit | UL94 class HB, DIN IEC 60695-11-10 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzmassenflussrate | 39 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 39 g/10min | DIN EN ISO 1133 | 230°C/2.16kg |
Schmelzvolumenflussrate | 37 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 37 cm³/10min | DIN EN ISO 1133 | 230°C/2.16kg |
Schrumpfung | 1.4 % Show Supplier Material materials with Schrumpfung of 1.4 % | DIN EN ISO 294-4 | |
1.54 % Show Supplier Material materials with Schrumpfung of 1.54 % | DIN EN ISO 294-4 | Transverse |
Technological properties
Property | ||
---|---|---|
Certifications | Explanation of food contact according to FDA and EU 10/2011 | |
Color | Blue | |
Detectability | Inductive: 6 mm Al, X-Ray detectable: 3.5 mm Al | |
Fillers | Detectable Filler | |
Processing methods | Permissible residual moisture content (%): 0.1, drying temperature (°C): 100, drying time (h): 2, mould temperature (°C): 100, material temperature (°C): 250, cylinder/processing temperature (°C): 260 |