Allgemein
Property | Value |
---|---|
Dichte | 6.5 g/cm³ Show Supplier Material materials with Dichte of 6.5 g/cm³ |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 2.8 % Show Supplier Material materials with Dehnung of 2.8 % | |
Härte, Vickers | 280 - 320 [-] Show Supplier Material materials with Härte, Vickers of 280 - 320 [-] | HV 0.5 |
Maximal zulässige Belastung | 370 MPa Show Supplier Material materials with Maximal zulässige Belastung of 370 MPa | |
450 MPa Show Supplier Material materials with Maximal zulässige Belastung of 450 MPa |
Technological properties
Property | ||
---|---|---|
Application areas | Mechanical, Aerospace, Biomedical | |
Other | Diameter 10 mm by 2-7 mm disks. Diameter 15 mm by 2-7 mm disks. 20 x 10 x 2 to 8 mm heigh. Special shapes upon request. | |
Processing methods | E-Forged™ from powders |