Allgemein
Property | Value |
---|---|
Dichte | 10.1 g/cm³ Show Supplier Material materials with Dichte of 10.1 g/cm³ |
Porosität | 3 % Show Supplier Material materials with Porosität of 3 % |
Mechanisch
Property | Value | Comment |
---|---|---|
Härte, Vickers | 187 - 189 [-] Show Supplier Material materials with Härte, Vickers of 187 - 189 [-] | HV 0.2 |
Elektrisch
Property | Value |
---|---|
spezifischer Widerstand | 4.01e-08 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.01e-08 Ω·m |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical contacts | |
Other | Diameter 10 mm by 2-10 mm disks. Diameter 15 mm by 2-10 mm disks. 20 x 10 x 2 to 6 mm heigh. Special shapes upon request. | |
Processing methods | E-Forged™ from powders |