Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 17.8 - 18.2 g/cm³ Show Supplier Material materials with Dichte of 17.8 - 18.2 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 3 - 25 % Show Supplier Material materials with Dehnung of 3 - 25 % |
Härte, Vickers, 10 | 23.0 °C | 290 - 340 [-] Show Supplier Material materials with Härte, Vickers, 10 of 290 - 340 [-] |
Zugfestigkeit | 23.0 °C | 750 - 950 MPa Show Supplier Material materials with Zugfestigkeit of 750 - 950 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 2E-3 % Show Supplier Material materials with Aluminium of 2E-3 % | Max. | |
Andere | 5 % Show Supplier Material materials with Andere of 5 % | Ni+Fe | |
Arsen | 2E-3 % Show Supplier Material materials with Arsen of 2E-3 % | Max. | |
Chrom | 2E-3 % Show Supplier Material materials with Chrom of 2E-3 % | Max. | |
Kalium | 1E-3 % Show Supplier Material materials with Kalium of 1E-3 % | Max. | |
Kalzium | 2E-3 % Show Supplier Material materials with Kalzium of 2E-3 % | Max. | |
Kobalt | 3E-3 % Show Supplier Material materials with Kobalt of 3E-3 % | Max. | |
Kohlenstoff | 5E-3 % Show Supplier Material materials with Kohlenstoff of 5E-3 % | Max. | |
Kupfer | 1E-3 % Show Supplier Material materials with Kupfer of 1E-3 % | Max. | |
Magnesium | 2E-3 % Show Supplier Material materials with Magnesium of 2E-3 % | Max. | |
Molybdän | 5E-3 % Show Supplier Material materials with Molybdän of 5E-3 % | Max. | |
Natrium | 2E-3 % Show Supplier Material materials with Natrium of 2E-3 % | Max. | |
Schwefel | 2E-3 % Show Supplier Material materials with Schwefel of 2E-3 % | Max. | |
Silizium | 3E-3 % Show Supplier Material materials with Silizium of 3E-3 % | Max. | |
Wolfram | balance |
Technological properties
Property | ||
---|---|---|
Application areas | Material to balance rotating systems (aviation, radar, crankshafts etc.); Radiation protection material (Shielding parts for medical diagnostic and radiation therapy); Material for tool holders and high speed spindles; Upsetting tools; Moulds for aluminium, magnesium, zinc and copper high pressure die casting |