Description

APTIV® 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.


APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom.


APTIV 1000 has a unique combination of properties providing high temperature performance, lightweight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen-free and ease of processing makes APTIV films a technology enabler for our customers and end users.

Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Abmessung

PropertyValue

Dicke

0.25 mm

Show Material materials with Dicke of 0.25 mm

Mechanisch

PropertyTemperatureValueComment

Dehnung

23.0 °C

150 %

Show Material materials with Dehnung of 150 %

ISO 527

Dehnung, transversal

23.0 °C

150 %

Show Material materials with Dehnung, transversal of 150 %

ISO 527

Elastizitätsmodul

23.0 °C

2.3 GPa

Show Material materials with Elastizitätsmodul of 2.3 GPa

ISO 527

Elastizitätsmodul, transversal

23.0 °C

2.3 GPa

Show Material materials with Elastizitätsmodul, transversal of 2.3 GPa

ISO 527

Zugfestigkeit

23.0 °C

110 MPa

Show Material materials with Zugfestigkeit of 110 MPa

ISO 527

Zugfestigkeit, transversal

23.0 °C

110 MPa

Show Material materials with Zugfestigkeit, transversal of 110 MPa

ISO 527

Elektrisch

PropertyTemperatureValueComment

Durchschlagfestigkeit

23.0 °C

70 kV/mm

Show Material materials with Durchschlagfestigkeit of 70 kV/mm

ASTM D149 (6.25mm electrode)

Durchschlagspannung

23.0 °C

17.5 kV

Show Material materials with Durchschlagspannung of 17.5 kV

ASTM D149 (6.25mm electrode)

Technological properties

Property
Application areas

Electrical insulation, pressure sensitive tapes, printed circuit substrates, high temperature labels, washers in high speed motors, washers in mobile phone hinges, flexible surface heaters, aerospace insulation, pressure sensor membranes, acoustic speaker diaphragms, capacitors, composites, proven temperature resistance to use of lead free solders

Certifications

APTIV® film is FDA and EU approved for food contact and is RoHS and 3A Sanitary Standards compliant.

Other

The key features are: High heat resistance, excellent tribological properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent barrier properties, excellent acoustic properties, high purity, lightweight, recyclable, easy to process

Processing methods

Can be laminated to other materials, thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated.