APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.


APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom.


APTIV 1100 has a unique combination of properties providing high temperature performance, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen-free and ease of processing makes APTIV films a technology enabler for our customers and end users.


APTIV 1100 series provides a higher modulus and lower coefficient of linear thermal expansion over the APTIV 1000 series.

Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Abmessung

PropertyValue

Dicke

0.05 mm

Show Material materials with Dicke of 0.05 mm

Mechanisch

PropertyTemperatureValueComment

Dehnung

23.0 °C

10 %

Show Material materials with Dehnung of 10 %

ISO 527

Dehnung, transversal

23.0 °C

10 %

Show Material materials with Dehnung, transversal of 10 %

ISO 527

Elastizitätsmodul

23.0 °C

5.5 GPa

Show Material materials with Elastizitätsmodul of 5.5 GPa

ISO 527

Elastizitätsmodul, transversal

23.0 °C

4.5 GPa

Show Material materials with Elastizitätsmodul, transversal of 4.5 GPa

ISO 527

Zugfestigkeit

23.0 °C

90 MPa

Show Material materials with Zugfestigkeit of 90 MPa

ISO 527

Zugfestigkeit, transversal

23.0 °C

90 MPa

Show Material materials with Zugfestigkeit, transversal of 90 MPa

ISO 527

Technological properties

Property
Application areas

Electrical insulation, printed circuit substrates, high temperature labels, flexible surface heaters, proven temperature resistance to use of lead free solders, acoustic speaker diaphragms, pressure sensor membranes

Certifications

APTIV® film is FDA and EU approved for food contact and is RoHS compliant.

Other

The key features are: High heat resistance, broad chemical resistance, excellent barrier properties, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties, high purity, lightweight, recyclable, easy to process. The APTIV 1100 series offers an improved thermal conductivity over APTIV 1000 films.

Processing methods

Can be laminated to other materials, thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated.